logo

X46cr13/4Cr13 Extruded Fin Tube and Aluminum Fin Tube with 300°C Max Working Temperature and 18,500mm Tube Length

Place of Origin:China
Brand Name:DELLOK Yonghui
Certification:Ce
Model Number:X46cr13/4Cr13
Minimum Order Quantity:1 meter
Price:$10 - 100 /Piece/Pieces
Payment Terms:T/T, L/C, D/A, D/P, Western Union,
Supply Ability:10000 Pieces Monthly
Product Details
Highlight:

Aluminium Extruded Fin Tube

,

Finned Aluminum Extrusion Tube

Raw Material ::: X46cr13/4Cr13
Trademark:: DELLOK
HS Code :: 8436990000
Applicable Materials Shape :: Powder
Production Capacity:: 5000 Pieces/Year
Origin:: Yangzhou Jiangsu China
Application: Air Cooler/Condenser/Evaporator
Fin Coating: Powder Coating/Anodizing/Electrophoresis
Fin Height: 5~16 (mm)
Fin Pitch: 2-20mm
Fin Surface: Smooth/Embossed/Serrated
Fin Thickness: 0.3~1.2 (mm)
Fin Type: Extruded
Material: Aluminum/Copper/Stainless Steel
Max Working Pressure: 0.6-3.0MPa
Max Working Temperature: 300°C
Shape: Round/Square/Rectangular
Tube Coating: Powder Coating/Anodizing/Electrophoresis
Tube Diameter: 6-50mm
Tube Length: ≤18,500 (mm)
Tube Thickness: 0.2-2.0mm
Product Description
Product Overview

DELLOK Aluminum Fin Rolled Exchanger Heat Finned Tube is a bimetallic extruded fin tube manufactured by inserting a base tube into an aluminum tube and directly extruding the aluminum into the desired fin specification. The tight contact between fin and tube surface improves heat transfer efficiency while providing considerable corrosion protection to the base tube.

Extruded aluminum finned tube with tightly bonded aluminum fins on a base tube
Extruded aluminum finned tube
About DELLOK (YONGHUI)

DELLOK (YONGHUI RADIATING PIPE MANUFACTURING CO., LTD.) was established in 2002 and is located in Jiangsu, China. After years of development, the company now holds 66 million yuan in fixed assets, employs more than 200 people, and retains 33 technical staff.

Our production capabilities include:

  • 4 aluminum processing production lines with an annual processing capacity of more than 20,000 tons
  • 5 tube-drawing production lines
  • 47 fin tube production lines
  • 1 imported production line from the American brand McElroy
  • Annual production capacity of 12 million meters and above

Quality is the eternal pursuit of our company. Meticulous workmanship, a standardized management system, and systematic quality assurance are Dellok (YONGHUI)'s best commitment to quality. Quality control is not limited to final inspection — it runs throughout the entire production process. We implement a complete quality control and assurance system: each batch of pipes is sampled and tested, and records are kept as a quality guarantee for the final product.

Product Description

Bimetallic extruded fin tubes use a base tube inserted into an aluminum tube, with the aluminum directly extruded into the desired fin specification. The fin and tube surfaces are in tight contact, improving heat transfer efficiency and giving considerable corrosion protection to the base tube.

Close-up of extruded aluminum tubing showing integrated fin structure
Extruded aluminum tubing
Manufacturing Process

Extruded fin tubes are produced by compressing an aluminum tube, or sleeve, onto the base tube. The bloom is exposed to very high pressures, which essentially "grows" the fins into the final fin profiles. This process creates an excellent, strong joint with great resistance (fin stiffness) as well as exceptional heat transfer capabilities (longevity, temperature range).

The advantages of extruded fin tubes include full protection of the bare tube against corrosion and high mechanical strength of the fin. Extruded finned tubes provide the most stable performance over time compared with other fin types. The fin is rolled from an outer aluminum tube using pressure to create a rolled "pressure bond" between the liner tube and fins. The aluminum fin material completely encloses the tube, except at the ends where a tube coating can be applied.

Extruded fin tube with rigid aluminum fins bonded to the base tube
Extruded fin tube
Advantages of Extruded Fin Tubes
Thermal Performance

The bonding of the outer and inner tubes removes the risk of loss of contact with the aluminum due to thermal stress. Maximum operating temperature is 250°C. The transfer coefficient remains steady. Additionally, because the outer sleeve is continuous, no electrolytic couple is created.

Mechanical Performance

The fins are more rigid and withstand handling shocks better compared with type "G" and "L" fins.

Extruded finned tubes arranged in a bundle for heat exchanger use
Extruded finned tubes
Properties
  • Manufacturing Process: Cold extrusion
  • Fin-to-Tube Bond: Excellent
  • Heat Transfer Efficiency: Excellent
  • Mechanical Resistance: Excellent — can be frequently cleaned with high-pressure jets unlike other fin tubes, reducing downtime and increasing overall life
  • Corrosion Protection: Excellent protection for the base tube, since the aluminum entirely covers the base tube (except bare ends)
  • Temperature Range: Up to a maximum of 300°C
Extruded finned tube detail showing fin-to-tube bonding
Extruded finned tube
Applications
  • Petroleum, chemical, and petrochemical industries
  • Natural gas treatment
  • Steel industry: blast furnace and converter cooling systems
  • Power generation: steam turbine exhaust condensing
    • Contact condensing with cooling of circulating condensate
    • Fossil and nuclear power plants
  • Air conditioning (freon, ammonia, propane)
  • Incineration of household refuse
  • Compressor coolers, etc.
Aluminum extruded tubing used in industrial heat exchange applications
Aluminum extruded tubing
Specifications
Parameter Metric Imperial
Tube OD 10–51 mm 0.4"–2"
Tube Wall Thickness 1.65–3.0 mm 0.065"–0.118"
Tube Length ≤ 18,500 mm ≤ 60.7 ft
Fin Thickness 0.3–1.2 mm 0.012"–0.047"
Fin Height 5–16 mm 0.2"–0.63"
Fin Pitch 100–555 mm 3–14 FPI
Fin Type Extruded
Material Combinations
Component Available Materials
Fin Material Aluminum (most common grades: Alu. 1100, Alu. 1060, Alu. 6063); Copper
Tube Material C.S. (most common grades: A179, A192, SA210 GrA1/C, A106 Gr B);
S.S. (most common grades: TP304, 316, 321, 347, A789);
Copper (most common grades: UNS12200, 14200, 70600, CuNi70/30, CuNi 90/10);
Titanium (most common grade: B338Gr2)
Applied Temperature 300°C
Type of Service Medium temperature, severe atmospheric corrosive environment
Product Details

Fin Type: Extruded fin tube
Tube Material: Copper, copper nickel, stainless steel, titanium, etc.
Fin Material: Copper, aluminum

Aluminum extruded finned tube with base tube fully covered by aluminum sleeve
Aluminum extruded finned tube

Aluminum extruded finned tubes, also called "integral finned tubes," use the form of a base tube covered with an aluminum tube (the base tube can be carbon steel, stainless steel, or copper) through machine extrusion, forming a tube fin. The fin base and the tube outer wall are close fitting, which allows the finned tubes to achieve a high heat transfer coefficient and strong heat transfer performance.

Extruded finned tubes can be made of iron, copper, or aluminum tube by compound rolling. They offer the advantages of tight bonding, small thermal resistance, good heat transfer performance, high strength, small flow loss, strong anti-corrosion performance, resistance to deformation under long-term hot and cold working conditions, and long working life.

Extruded finned tube cross-section showing bimetallic construction
Extruded finned tube
Extruded Finned Tube Manufacturing Process

The production flow is: pipe line → compressing or rolling → strip peeling → washing → pressure test → blast blowing → packaging.

The extruded fin tube is formed from a bimetallic tube consisting of an aluminum outer tube and an inner tube of almost any material. The fin is formed by rolling the material from the outside of the outer tube to provide an integrated fin with excellent heat transfer performance and long life. The extruded fins provide excellent corrosion protection for the base tube.

The production method of the composite finned tube mainly uses the extrusion method: the bimetallic composite tube is lined with a mandrel, and driven by the rotation of the roller blade, the composite tube is processed on the outer surface through the cavity formed by the rolling groove and the core head to produce fins. The heat transfer tube produced by this method is an organic whole with its outer tube and fins, so there is no contact heat loss, and it delivers good performance and high heat transfer efficiency.

Extruded aluminum tube with integrated fins produced by cold extrusion
Extruded aluminum tube
Frequently Asked Questions
Q: What is your lead time for production?

A: Generally, samples need 1–3 days; mass production needs 15–30 days, also depending on your request.

Q: What is the warranty for your products?

A: We provide a one-year warranty for the products.

Q: What payment terms do you accept?

A: Trade assurance, TT, Western Union.

Q: What are the modes of transportation for the machines?

A: Air freight, sea freight, express delivery, etc. We will choose the most suitable transportation method according to your requirements.

You May Also Like
Quality TP304L Resistance Welded Perforated Fins Longitudinal Finned Tube for Heat Exchangers factory

TP304L Resistance Welded Perforated Fins Longitudinal Finned Tube for Heat Exchangers

TP304L Longitudinal Finned Tube The TP304L Longitudinal Finned Tube is a high-performance heat transfer component designed for demanding industrial applications. Manufactured with precision resistance welding, longitudinal fins are securely bonded to the core plain tube, delivering superior thermal ...
Quality DELLOK YONGHUI Cold Drawn Carbon Steel Fin Height 16.5mm Extruded Fin Tube factory

DELLOK YONGHUI Cold Drawn Carbon Steel Fin Height 16.5mm Extruded Fin Tube

Cold Drawn Seamless Carbon Steel A179 Extruded Fin Tube A213 T22 , OD1' X 54' Length X 10FPI X Alu 1100 Fins , extruded high fin cooling tube Tube Type:Seamless (Cold Drawn) Ends:Plain ends or bevel ends. Surface protection:black painting,anti-rust oil or varnish. Introduction: A smooth core tube is ...
Quality DELLOK YONGHUI Chemical Industry Stud SA335 P91 Carbon Steel Seamless Tube factory
video

DELLOK YONGHUI Chemical Industry Stud SA335 P91 Carbon Steel Seamless Tube

Chemical Industry Stud SA335 P91 Carbon Steel Seamless Tube SA335 P11 / P22 / P91 from BaoSteel , NPS 4'(114.3mm) studded pin heating tubes ASTM A335/A335M: Seamless Ferritic Alloy-Steel Pipe for High-Temperature Service Product Details Material: Carbon, stainless, and alloy steels. Tube details: ...
Quality High Performance Copper Integral Low Fin Tube for Air Conditioning and Heat Exchanger Applications factory

High Performance Copper Integral Low Fin Tube for Air Conditioning and Heat Exchanger Applications

Product Overview DELLOK High Performance Copper Integral Finned Tube Low fin tubes are formed by rolling short fins directly into the tube wall, greatly increasing the surface area compared to a smooth tube. Because the fins are integral to the tube wall, the outside diameter of the finned section ...
Contact Us
you can contact us at anytime!